Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Stress | 97.3 MPa @Strain 1.28 %, Temperature 23.0 °C |
14100 psi @Strain 1.28 %, Temperature 73.4 °F |
DAM; ISO 11403-1 -2 |
DuPont Performance Polymers Zytel® 70G25HSL NC010 Nylon 66
(Unverified Data**) 25% Glass Reinforced Heat Stabilized Polyamide 66 Zytel 70G25HSL NC010 is a 25% glass fiber reinforced heat stabilized polyamide 66 resin for injection molding.Information provided by DuPont Perform.. |