Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Stress | 66.9 MPa @Strain 0.420 %, Temperature -40.0 °C |
9700 psi @Strain 0.420 %, Temperature -40.0 °F |
DAM; ISO 11403-1 -2 |
DuPont Performance Polymers Zytel® 77G43L NC010 Nylon 612
(Unverified Data**) 43% Glass Reinforced Polyamide 612Zytel 77G43L NC010 is a 43% glass fiber reinforced polyamide 612 resin for injection molding.Information provided by DuPont Performance Polymers |