Tensile Stress 68.01 MPa

@Strain 0.800 %,
Temperature 0.000 °C
9864 psi

@Strain 0.800 %,
Temperature 32.0 °F
DAM; ISO 11403-1 -2
DuPont Performance Polymers Minlon® 10B40 NC010 Nylon 66  (Unverified Data**)
40% Mineral Reinforced Polyamide 66Minlon 10B40 NC010 is a 40% mineral reinforced polyamide 66 resin for injection molding.Information provided by DuPont Performance Polymers