Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Stress | 68.33 MPa @Strain 6.04 %, Temperature 40.0 °C |
9910 psi @Strain 6.04 %, Temperature 104 °F |
DAM; ISO 11403-1 -2 |
DuPont Performance Polymers Minlon® 73M40 NC010 Nylon 6
(Unverified Data**) 40% Mineral Reinforced Polyamide 6 Minlon 73M40 NC010 is a 40% mineral reinforced heat stabilized polyamide 6 resin for injection molding. It has isotropic properties and low warpage.Information pro.. |
|||
Tensile Stress | 68.3 MPa @Strain 0.900 %, Temperature 40.0 °C |
9910 psi @Strain 0.900 %, Temperature 104 °F |
ISO 11403-1 -2 |
DuPont Performance Polymers Rynite® GW520CS NC010 Polyethylene Terephthalate (PET) 20% Glass Reinforced Flame Retardant Polyethylene Terephthalate with Improved Glow Wire Performance Rynite GW520CS NC010 is a 20% glass fiber reinforced flame retardant color stabilized modified pol.. |