Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Clash Berg Modulus | 0.310 GPa @Temperature -10.0 °C |
45.0 ksi @Temperature 14.0 °F |
ASTM D1043 |
PolyOne Geon™ Vinyl Flexible A5DM0 Polyvinyl Chloride, Flexible (PVC, Flexible) Recommended for interior applications.Information provided by PolyOne |
|||
Clash Berg Modulus | 0.310 GPa @Temperature -40.0 °C |
45.0 ksi @Temperature -40.0 °F |
ASTM D1043 |
PolyOne Geon™ Vinyl Flexible A6500 Polyvinyl Chloride, Flexible (PVC, Flexible) Recommended for interior applications.Information provided by PolyOne |
|||
Clash Berg Modulus | 0.310 GPa @Temperature -52.0 °C |
45.0 ksi @Temperature -61.6 °F |
ASTM D1043 |
PolyOne Geon™ Vinyl Flexible A7000 Polyvinyl Chloride, Flexible (PVC, Flexible) Interior compound used primarily in transparent applications. This product is registered under UL 94 HB specifications @ 3.0 and 1.5 mm. thickness and all colors.Information provided by PolyOne |
|||
Clash Berg Modulus | 0.310 GPa @Temperature -47.0 °C |
45.0 ksi @Temperature -52.6 °F |
ASTM D1043 |
PolyOne Geon™ Vinyl Flexible A75G0 Polyvinyl Chloride, Flexible (PVC, Flexible) Recommended for interior applications.Information provided by PolyOne |
|||
Clash Berg Modulus | 0.310 GPa @Temperature -22.0 °C |
45.0 ksi @Temperature -7.60 °F |
ASTM D1043 |
PolyOne Geon™ Vinyl Flexible A75M1 Trans 9000 Polyvinyl Chloride, Flexible (PVC, Flexible) This compound is certified for fuel hose applications(R1 Type B Class 1)under SAE J 1527 requirements.Information provided by PolyOne |
|||
Clash Berg Modulus | 0.310 GPa @Temperature -42.0 °C |
45.0 ksi @Temperature -43.6 °F |
ASTM D1043 |
PolyOne Geon™ Vinyl Flexible A8000 Polyvinyl Chloride, Flexible (PVC, Flexible) Recommended for interior applications.Information provided by PolyOne |
|||
Clash Berg Modulus | 0.310 GPa @Temperature -20.0 °C |
45.0 ksi @Temperature -4.00 °F |
ASTM D1043 |
PolyOne Geon™ Vinyl Flexible A8500 Polyvinyl Chloride, Flexible (PVC, Flexible) Recommended for interior applications.Information provided by PolyOne |
|||
Clash Berg Modulus | 0.310 GPa @Temperature -24.0 °C |
45.0 ksi @Temperature -11.2 °F |
ASTM D1043 |
PolyOne Geon™ Vinyl Flexible A9000 Polyvinyl Chloride, Flexible (PVC, Flexible) Recommended for interior applications.Information provided by PolyOne |
|||
Clash Berg Modulus | 0.310 GPa @Temperature -23.0 °C |
45.0 ksi @Temperature -9.40 °F |
ASTM D1043 |
PolyOne Geon™ Vinyl Flexible A90F1 Polyvinyl Chloride, Flexible (PVC, Flexible) Recommended for interior applications.Information provided by PolyOne |
|||
Clash Berg Modulus | 0.310 GPa @Temperature -57.0 °C |
45.0 ksi @Temperature -70.6 °F |
ASTM D1043 |
PolyOne Geon™ Vinyl Flexible B6000 Polyvinyl Chloride, Flexible (PVC, Flexible) Information provided by PolyOne |
|||
Clash Berg Modulus | 0.310 GPa @Temperature 2.00 °C |
45.0 ksi @Temperature 35.6 °F |
ASTM D1043 |
PolyOne Geon™ Vinyl Flexible B6D00 Polyvinyl Chloride, Flexible (PVC, Flexible) Information provided by PolyOne |
|||
Clash Berg Modulus | 0.310 GPa @Temperature -36.0 °C |
45.0 ksi @Temperature -32.8 °F |
ASTM D1043 |
PolyOne Geon™ Vinyl Flexible B6DT0 Polyvinyl Chloride, Flexible (PVC, Flexible) Information provided by PolyOne |
|||
Clash Berg Modulus | 0.310 GPa @Temperature -43.0 °C |
45.0 ksi @Temperature -45.4 °F |
ASTM D1043 |
PolyOne Geon™ Vinyl Flexible B7500 Polyvinyl Chloride, Flexible (PVC, Flexible) Information provided by PolyOne |
|||
Clash Berg Modulus | 0.310 GPa @Temperature -34.0 °C |
45.0 ksi @Temperature -29.2 °F |
ASTM D1043 |
PolyOne Geon™ Vinyl Flexible C8500 Polyvinyl Chloride, Flexible (PVC, Flexible) Information provided by PolyOne |
|||
Clash Berg Modulus | 0.310 GPa @Temperature -36.0 °C |
45.0 ksi @Temperature -32.8 °F |
ASTM D1043 |
PolyOne Geon™ Vinyl Flexible C90A0 Polyvinyl Chloride, Flexible (PVC, Flexible) Information provided by PolyOne |
|||
Clash Berg Modulus | 0.310 GPa @Temperature -26.0 °C |
45.0 ksi @Temperature -14.8 °F |
ASTM D1043 |
PolyOne Geon™ Vinyl Flexible C90B1 Polyvinyl Chloride, Flexible (PVC, Flexible) Information provided by PolyOne |
|||
Clash Berg Modulus | 0.310 GPa @Temperature -26.0 °C |
45.0 ksi @Temperature -14.8 °F |
ASTM D1043 |
PolyOne Geon™ Vinyl Flexible C90UB Polyvinyl Chloride, Flexible (PVC, Flexible) Information provided by PolyOne |
|||
Clash Berg Modulus | 0.310 GPa @Temperature -28.0 °C |
45.0 ksi @Temperature -18.4 °F |
ASTM D1043 |
PolyOne Geon™ Vinyl Flexible D75M0 Polyvinyl Chloride, Flexible (PVC, Flexible) Information provided by PolyOne |
|||
Clash Berg Modulus | 0.310 GPa @Temperature -41.0 °C |
45.0 ksi @Temperature -41.8 °F |
ASTM D1043 |
PolyOne Geon™ Vinyl Flexible D8000 Polyvinyl Chloride, Flexible (PVC, Flexible) Information provided by PolyOne |
|||
Clash Berg Modulus | 0.310 GPa @Temperature -22.0 °C |
45.0 ksi @Temperature -7.60 °F |
ASTM D1043 |
PolyOne Geon™ Vinyl Flexible D80M0 Polyvinyl Chloride, Flexible (PVC, Flexible) Information provided by PolyOne |
|||
Clash Berg Modulus | 0.310 GPa @Temperature -33.0 °C |
45.0 ksi @Temperature -27.4 °F |
ASTM D1043 |
PolyOne Geon™ Vinyl Flexible B4DC1 Polyvinyl Chloride, Flexible (PVC, Flexible) Information provided by PolyOne |
|||
Clash Berg Modulus | 0.310 GPa @Temperature -59.0 °C |
45.0 ksi @Temperature -74.2 °F |
ASTM D1043 |
PolyOne Geon™ Vinyl Flexible B5500 Polyvinyl Chloride, Flexible (PVC, Flexible) Information provided by PolyOne |
|||
Clash Berg Modulus | 0.310 GPa @Temperature -28.0 °C |
45.0 ksi @Temperature -18.4 °F |
ASTM D1043 |
PolyOne Geon™ Vinyl Flexible B5D02 Polyvinyl Chloride, Flexible (PVC, Flexible) Information provided by PolyOne |
|||
Clash Berg Modulus | 0.310 GPa @Temperature -26.0 °C |
45.0 ksi @Temperature -14.8 °F |
ASTM D1043 |
PolyOne Geon™ Vinyl Flexible B9000 Polyvinyl Chloride, Flexible (PVC, Flexible) Information provided by PolyOne |
|||
Clash Berg Modulus | 0.310 GPa @Temperature -14.0 °C |
45.0 ksi @Temperature 6.80 °F |
ASTM D1043 |
PolyOne Geon™ Vinyl Flexible C5D01 Polyvinyl Chloride, Flexible (PVC, Flexible) Information provided by PolyOne |
|||
Clash Berg Modulus | 0.310 GPa @Temperature -52.0 °C |
45.0 ksi @Temperature -61.6 °F |
ASTM D1043 |
PolyOne Geon™ Vinyl Flexible C6500 Polyvinyl Chloride, Flexible (PVC, Flexible) Information provided by PolyOne |
|||
Clash Berg Modulus | 0.310 GPa @Temperature -43.0 °C |
45.0 ksi @Temperature -45.4 °F |
ASTM D1043 |
PolyOne Geon™ Vinyl Flexible C70A0 Polyvinyl Chloride, Flexible (PVC, Flexible) Information provided by PolyOne |
|||
Clash Berg Modulus | 0.310 GPa @Temperature -42.0 °C |
45.0 ksi @Temperature -43.6 °F |
ASTM D1043 |
PolyOne Geon™ Vinyl Flexible C7500 Polyvinyl Chloride, Flexible (PVC, Flexible) Information provided by PolyOne |
|||
Clash Berg Modulus | 0.310 GPa @Temperature -42.0 °C |
45.0 ksi @Temperature -43.6 °F |
ASTM D1043 |
PolyOne Geon™ Vinyl Flexible C75A0 Polyvinyl Chloride, Flexible (PVC, Flexible) Information provided by PolyOne |
|||
Clash Berg Modulus | 0.310 GPa @Temperature -23.0 °C |
45.0 ksi @Temperature -9.40 °F |
ASTM D1043 |
PolyOne Geon™ Vinyl Flexible D7000 Polyvinyl Chloride, Flexible (PVC, Flexible) Information provided by PolyOne |