Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Clash Berg Modulus | 0.310 GPa @Temperature -13.0 °C |
45.0 ksi @Temperature 8.60 °F |
ASTM D1043 |
PolyOne Geon™ Vinyl Flexible A4D00 Polyvinyl Chloride, Flexible (PVC, Flexible) Information provided by PolyOne |
|||
Clash Berg Modulus | 0.310 GPa @Temperature -10.0 °C |
45.0 ksi @Temperature 14.0 °F |
ASTM D1043 |
PolyOne Geon™ Vinyl Flexible A5DM0 Polyvinyl Chloride, Flexible (PVC, Flexible) Recommended for interior applications.Information provided by PolyOne |
|||
Clash Berg Modulus | 0.310 GPa @Temperature -11.0 °C |
45.0 ksi @Temperature 12.2 °F |
ASTM D1043 |
PolyOne Geon™ Vinyl Flexible A5DU0 Polyvinyl Chloride, Flexible (PVC, Flexible) Recommended for interior applications.Information provided by PolyOne |
|||
Clash Berg Modulus | 0.310 GPa @Temperature -40.0 °C |
45.0 ksi @Temperature -40.0 °F |
ASTM D1043 |
PolyOne Geon™ Vinyl Flexible A6500 Polyvinyl Chloride, Flexible (PVC, Flexible) Recommended for interior applications.Information provided by PolyOne |
|||
Clash Berg Modulus | 0.310 GPa @Temperature -20.0 °C |
45.0 ksi @Temperature -4.00 °F |
ASTM D1043 |
PolyOne Geon™ Vinyl Flexible A8500 Polyvinyl Chloride, Flexible (PVC, Flexible) Recommended for interior applications.Information provided by PolyOne |
|||
Clash Berg Modulus | 0.310 GPa @Temperature -24.0 °C |
45.0 ksi @Temperature -11.2 °F |
ASTM D1043 |
PolyOne Geon™ Vinyl Flexible A90U2 Polyvinyl Chloride, Flexible (PVC, Flexible) GENERAL PURPOSE CLEAR PVC COMPOUND WITH LOW LEVEL OF U.V. INHIBITOR, to be used only in interior applications.Information provided by PolyOne |
|||
Clash Berg Modulus | 0.310 GPa @Temperature -20.0 °C |
45.0 ksi @Temperature -4.00 °F |
ASTM D1043 |
PolyOne Geon™ Vinyl Flexible B5DU0 Polyvinyl Chloride, Flexible (PVC, Flexible) Information provided by PolyOne |
|||
Clash Berg Modulus | 0.310 GPa @Temperature -57.0 °C |
45.0 ksi @Temperature -70.6 °F |
ASTM D1043 |
PolyOne Geon™ Vinyl Flexible B6000 Polyvinyl Chloride, Flexible (PVC, Flexible) Information provided by PolyOne |
|||
Clash Berg Modulus | 0.310 GPa @Temperature -55.0 °C |
45.0 ksi @Temperature -67.0 °F |
ASTM D1043 |
PolyOne Geon™ Vinyl Flexible B65F1 Polyvinyl Chloride, Flexible (PVC, Flexible) Information provided by PolyOne |
|||
Clash Berg Modulus | 0.310 GPa @Temperature 2.00 °C |
45.0 ksi @Temperature 35.6 °F |
ASTM D1043 |
PolyOne Geon™ Vinyl Flexible B6D00 Polyvinyl Chloride, Flexible (PVC, Flexible) Information provided by PolyOne |
|||
Clash Berg Modulus | 0.310 GPa @Temperature -36.0 °C |
45.0 ksi @Temperature -32.8 °F |
ASTM D1043 |
PolyOne Geon™ Vinyl Flexible B6DT0 Polyvinyl Chloride, Flexible (PVC, Flexible) Information provided by PolyOne |
|||
Clash Berg Modulus | 0.310 GPa @Temperature -32.0 °C |
45.0 ksi @Temperature -25.6 °F |
ASTM D1043 |
PolyOne Geon™ Vinyl Flexible B8500 Polyvinyl Chloride, Flexible (PVC, Flexible) Information provided by PolyOne |
|||
Clash Berg Modulus | 0.310 GPa @Temperature -32.0 °C |
45.0 ksi @Temperature -25.6 °F |
ASTM D1043 |
PolyOne Geon™ Vinyl Flexible B85B0 Polyvinyl Chloride, Flexible (PVC, Flexible) Information provided by PolyOne |
|||
Clash Berg Modulus | 0.310 GPa @Temperature -36.0 °C |
45.0 ksi @Temperature -32.8 °F |
ASTM D1043 |
PolyOne Geon™ Vinyl Flexible C90A0 Polyvinyl Chloride, Flexible (PVC, Flexible) Information provided by PolyOne |
|||
Clash Berg Modulus | 0.310 GPa @Temperature -26.0 °C |
45.0 ksi @Temperature -14.8 °F |
ASTM D1043 |
PolyOne Geon™ Vinyl Flexible C90UB Polyvinyl Chloride, Flexible (PVC, Flexible) Information provided by PolyOne |
|||
Clash Berg Modulus | 0.310 GPa @Temperature -41.0 °C |
45.0 ksi @Temperature -41.8 °F |
ASTM D1043 |
PolyOne Geon™ Vinyl Flexible D8000 Polyvinyl Chloride, Flexible (PVC, Flexible) Information provided by PolyOne |
|||
Clash Berg Modulus | 0.310 GPa @Temperature -22.0 °C |
45.0 ksi @Temperature -7.60 °F |
ASTM D1043 |
PolyOne Geon™ Vinyl Flexible D80M0 Polyvinyl Chloride, Flexible (PVC, Flexible) Information provided by PolyOne |
|||
Clash Berg Modulus | 0.310 GPa @Temperature -30.0 °C |
45.0 ksi @Temperature -22.0 °F |
ASTM D1043 |
PolyOne Geon™ Vinyl Flexible XV 3704 Polyvinyl Chloride, Flexible (PVC, Flexible) Information provided by PolyOne |
|||
Clash Berg Modulus | 0.310 GPa @Temperature -33.0 °C |
45.0 ksi @Temperature -27.4 °F |
ASTM D1043 |
PolyOne Geon™ Vinyl Flexible B4DC1 Polyvinyl Chloride, Flexible (PVC, Flexible) Information provided by PolyOne |
|||
Clash Berg Modulus | 0.310 GPa @Temperature -59.0 °C |
45.0 ksi @Temperature -74.2 °F |
ASTM D1043 |
PolyOne Geon™ Vinyl Flexible B5500 Polyvinyl Chloride, Flexible (PVC, Flexible) Information provided by PolyOne |
|||
Clash Berg Modulus | 0.310 GPa @Temperature -59.0 °C |
45.0 ksi @Temperature -74.2 °F |
ASTM D1043 |
PolyOne Geon™ Vinyl Flexible B550B Polyvinyl Chloride, Flexible (PVC, Flexible) Information provided by PolyOne |
|||
Clash Berg Modulus | 0.310 GPa @Temperature -28.0 °C |
45.0 ksi @Temperature -18.4 °F |
ASTM D1043 |
PolyOne Geon™ Vinyl Flexible B5D02 Polyvinyl Chloride, Flexible (PVC, Flexible) Information provided by PolyOne |
|||
Clash Berg Modulus | 0.310 GPa @Temperature -25.0 °C |
45.0 ksi @Temperature -13.0 °F |
ASTM D1043 |
PolyOne Geon™ Vinyl Flexible B5DG1 Polyvinyl Chloride, Flexible (PVC, Flexible) Information provided by PolyOne |
|||
Clash Berg Modulus | 0.310 GPa @Temperature -55.0 °C |
45.0 ksi @Temperature -67.0 °F |
ASTM D1043 |
PolyOne Geon™ Vinyl Flexible B65U0 Polyvinyl Chloride, Flexible (PVC, Flexible) Information provided by PolyOne |
|||
Clash Berg Modulus | 0.310 GPa @Temperature -14.0 °C |
45.0 ksi @Temperature 6.80 °F |
ASTM D1043 |
PolyOne Geon™ Vinyl Flexible B6DB1 Polyvinyl Chloride, Flexible (PVC, Flexible) Information provided by PolyOne |
|||
Clash Berg Modulus | 0.310 GPa @Temperature -43.0 °C |
45.0 ksi @Temperature -45.4 °F |
ASTM D1043 |
PolyOne Geon™ Vinyl Flexible C70A0 Polyvinyl Chloride, Flexible (PVC, Flexible) Information provided by PolyOne |
|||
Clash Berg Modulus | 0.310 GPa @Temperature -46.0 °C |
45.0 ksi @Temperature -50.8 °F |
ASTM D1043 |
PolyOne Geon™ Vinyl Flexible C70U0 Polyvinyl Chloride, Flexible (PVC, Flexible) Information provided by PolyOne |
|||
Clash Berg Modulus | 0.310 GPa @Temperature -46.0 °C |
45.0 ksi @Temperature -50.8 °F |
ASTM D1043 |
PolyOne Geon™ Vinyl Flexible C70UB Polyvinyl Chloride, Flexible (PVC, Flexible) Information provided by PolyOne |
|||
Clash Berg Modulus | 0.310 GPa @Temperature -42.0 °C |
45.0 ksi @Temperature -43.6 °F |
ASTM D1043 |
PolyOne Geon™ Vinyl Flexible C75A0 Polyvinyl Chloride, Flexible (PVC, Flexible) Information provided by PolyOne |
|||
Clash Berg Modulus | 0.310 GPa @Temperature -23.0 °C |
45.0 ksi @Temperature -9.40 °F |
ASTM D1043 |
PolyOne Geon™ Vinyl Flexible D7000 Polyvinyl Chloride, Flexible (PVC, Flexible) Information provided by PolyOne |