Polymer Property : Clash Berg Modulus = 0.483 GPa
Polymer Property :
Clash Berg Modulus =
0.483 GPa
Product List
Mechanical Properties
Tips:
30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties
Metric
English
Comments
Clash Berg Modulus
0.483
GPa
70.1
ksi
ASTM D1043
PolyOne Geon™ Vinyl Flexible 86273 Trans 002 Polyvinyl Chloride, Flexible (PVC, Flexible)
Information provided by PolyOne