Polymer Property : Flexural Strength = 10440 psi Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Flexural Strength 71.98 MPa
10440 psi
ASTM D790
Fiberfil® J-68/25/E/SD Polypropylene Copolymer, 25% Glass Fiber Reinforced, Chemically coupled, with static dissipation
Information provided by FIBERFIL Engineered Plastics
Flexural Strength 71.98 MPa
10440 psi
ASTM D790
Aclo Accucomp ABS ABS856BL High Flow Medium Impact Grade
Flexural Strength 71.98 MPa
10440 psi
ASTM D790
Aclo Accucomp ABS ABS892BL High Heat Grade
Flexural Strength 71.98 MPa
10440 psi
ASTM D790
Aclo Accutech Polypropylene Homopolymer HP0334G20CL Glass Reinforced Coupled
Flexural Strength 71.98 MPa
10440 psi
ASTM D790
Aclo Accutech Polypropylene Homopolymer HP0339G15M15CL Glass/Mineral Reinforced Coupled
Flexural Strength 71.98 MPa
10440 psi
ASTM D790
Aclo Accucomp ABS ABS892EL High Heat Grade