Polymer Property : Flexural Strength = 105.1 MPa Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Flexural Strength 105.1 MPa
15250 psi
ASTM D790
Spartech Polycast Cell Cast Acrylic
Description: Cell Cast AcrylicInformation provided by Spartech.
Flexural Strength 105.1 MPa
15250 psi
ASTM D790
Spartech Polycast Poly 76 (Mil-P-8184) Cell Cast Acrylic
Description: Cell Cast AcrylicInformation provided by Spartech.
Flexural Strength 105.1 MPa
15250 psi
ASTM D790
Spartech Polycast Poly 84 (Mil-P-8184) Cell Cast Acrylic
Description: Cell Cast AcrylicInformation provided by Spartech.
Flexural Strength 105.1 MPa
15250 psi
ASTM D790
Spartech Polycast Poly 900 (DTD-5592-UK) Cell Cast Acrylic
Description: Cell Cast AcrylicInformation provided by Spartech.
Flexural Strength 105.1 MPa
15250 psi
ASTM D790
Spartech Polycast Poly II (Mil-P-5425) Cell Cast Acrylic
Description: Cell Cast AcrylicInformation provided by Spartech.
Flexural Strength 105.1 MPa
15250 psi
ASTM D790
Spartech Polycast UF3 Cell Cast Acrylic
Description: Cell Cast AcrylicInformation provided by Spartech.
Flexural Strength 105.1 MPa
15250 psi
ASTM D790
Spartech Polycast UF4 Cell Cast Acrylic
Description: Cell Cast AcrylicInformation provided by Spartech.
Flexural Strength 105.1 MPa
15250 psi
ASTM D790
Spartech Polycast UF96 Cell Cast Acrylic
Description: Cell Cast AcrylicInformation provided by Spartech.
Flexural Strength 105.1 MPa
15250 psi
ASTM D790
Spartech Polycast UVT (Ultra-Violet Transmitting) Cell Cast Acrylic
Description: Cell Cast AcrylicInformation provided by Spartech.