Flexural Strength 11.5 MPa
1670 psi
ISO 178
Solvay TECHNYL® A 218 V15 PA66, 15% glass fiber, Conditioned
Description: Polyamide 66, reinforced with 15% of glass fiber, heat stabilized, for injection molding.Available in: Latin AmericaProduct Applications: TECHNYL® A 218 V15 is used in all sectors of..
Flexural Strength 11.5 MPa
1670 psi
SAE J949
Azdel SuperLite® SL550700-100 PP Resin Matrix / 55% Glass Fiber (2 mm Molded Thickness)
AZDEL SuperLite® SL550700-100 is a low pressure, thermoformable, thermoplastic composite of polypropylene and long chopped glass fibers. Usually combined with outer layers as needed for the applic..
Flexural Strength 11.5 MPa
1670 psi
SAE J949
Azdel SuperLite® SL550800-100 PP Resin Matrix / 55% Glass Fiber (1.5 mm Molded Thickness)
AZDEL SuperLite® SL550800-100 is a low pressure, thermoformable, thermoplastic composite of polypropylene and long chopped glass fibers. Usually combined with outer layers as needed for the applic..
Flexural Strength 11.5 MPa

@Thickness 19.0 mm
1670 psi

@Thickness 0.750 in
ASTM D790
3A Composites Core Materials AIREX® PXc.385 Fiber-Reinforced Structural Foam
AIREX® PXc is a closed-cell, fiber reinforced polymer foam with very high mechanical properties ideally suited as core material for structurally loaded sandwich applications. The sophisticated manu..