Mechanical Properties Metric English Comments
Flexural Strength 7.58 MPa
1100 psi
Cotronics Resbond™ 908 High Temperature Ceramic Adhesive, Moisture Proof
Flexural Strength 7.58 MPa
1100 psi
Cotronics Resbond™ 989 High Temperature, High Purity Alumina Adhesive, General Purpose