Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Strength | 112.0 MPa | 16250 psi | |
Master Bond EP112 Low Viscosity Heat Curing Cycloaliphatic Epoxy Adhesive Master Bond Polymer System EP112 is a solventless, low viscosity two component cycloaliphatic epoxy resin system which is specifically designed for high performance outdoor and indoor electrical & e.. |
|||
Flexural Strength | 112.0 MPa | 16240 psi | ASTM D790 |
Aclo Accutech ABS ABS833G20L Glass Reinforced |