Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Strength | 778 MPa | 113000 psi | ASTM D790 |
Quantum Composites AMC™ 8592 55% Carbon Fiber Reinforced SMC AMC™ 8592 is a chopped carbon fiber reinforced engineered structural composite molding compound. It is easily moldable and provides parts that are high strength, fatigue resistant, with high heat .. |