Mechanical Properties Metric English Comments
Flexural Strength 862 MPa
125000 psi
Transverse Rupture
Pacific Sintered Materials SS-410-R 410 Stainless Steel Powdered Metal
Magnetic stainless steel with high strength and good wearing properties.Equivalent MPIF Specification: SS-410-95All information provided by Pacific Sintered Metals.
Flexural Strength 862 MPa
125000 psi
Transverse Rupture
PSM Industries Pacific Sintered Metals 410 Stainless Steel SS-410-R Powdered Metal
Magnetic stainless steel with high strength and good wearing properties Equivalent MPIF Specification: SS-410-95Information Provided by Pacific Sintered Metals, a division of PSM Industries