Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Strength | 10.3 - 12.4 MPa | 1490 - 1800 psi | |
Ceradyne Thermo-Sil® Castable 220 Fused Silica Fused Silica is an excellent thermal insulator with an extremely low coefficient of thermal expansion. It is excellent for thermal shock applications. The key characteristics of this material are:Hi.. |
|||
Flexural Strength | 10.3 - 12.4 MPa | 1490 - 1800 psi | |
Ceradyne Thermo-Sil® Isomolded™ Fused Silica Fused Silica is an excellent thermal insulator with an extremely low coefficient of thermal expansion. It is excellent for thermal shock applications. The key characteristics of this material are:Hi.. |