Polymer Property : Flexural Strength = 1500 MPa Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Flexural Strength 1500 MPa
218000 psi
China Tungsten NT3 Titanium Carbonitride Alloy
Titanium carbonitride base alloy , also called cermets, with of high hardness, good red hard-ness and wear resistance, medium toughness, high  corrosion resistance to acids and alkalis and hi-tempe..
Flexural Strength 1500 MPa
218000 psi
China Tungsten NT6 Titanium Carbide and Nitride Based Carbides
Semi-finishing of low carbon steel, low alloy steel, gray cast iron, Si-AL alloy and finishing of stainless steel.Information provided by China Tungsten
Flexural Strength >= 1500 MPa
>= 218000 psi
China Tungsten YGR7 Tungsten Carbide with Rare Earth Additive
High hardness and strength, low friction, good wear resistance. Used as drawing dies for drawing and straightening of steels, non-ferrous metals and the alloy bars and tubings.Information provided b..
Flexural Strength 1500 MPa
218000 psi
China Tungsten YT6S Tungsten Carbide
Having the same wear resistance as YG6X but higher toughness. for tobacco cutters and rough and finish milling of cast iron.Information provided by China Tungsten
Flexural Strength 1500 MPa
218000 psi
China Tungsten YT772-2 Titanium Carbide and Nitride Based Carbides
Good wear resistance and better toughness, relative impact resistance , for intermittent turning and milling of cast iron and steel parts.Information provided by China Tungsten