Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Strength | 107 MPa | 15500 psi | ASTM D790 |
PolyOne LubriOne™ NN-000/20T Polyamide 66 (Nylon 66) LubriOne™ Lubricated and Wear-Resistant Compounds have been specifically formulated to be self-lubricating materials, offering low coefficient of friction and improved wear resistance properties. L.. |
|||
Flexural Strength | 107 MPa | 15500 psi | |
Quadrant EPP Nylatron® LFG PA 6 + oil, cast (ISO Data) Nylatron LFG (Lubricated Food Grade) is self-lubricating in the real meaning of the word, and has a FDA food contact compliant composition. The Nylatron LFG has been specially developed for non-lubr.. |
|||
Flexural Strength | 107 MPa | 15500 psi | ASTM D790 |
Fiberfil® J-60/30/E3 Polypropylene Homopolymer, 30% Glass Reinforced, Chemically coupled Information provided by FIBERFIL Engineered Plastics |
|||
Flexural Strength | 107 MPa | 15500 psi | ASTM D790 |
Fiberfil® J-60/30/F Polypropylene Homopolymer, 30% Glass Reinforced, Chemically coupled Information provided by FIBERFIL Engineered Plastics |
|||
Flexural Strength | 107 MPa | 15500 psi | ASTM D790 |
Fiberfil® M-2149 Polypropylene Homopolymer, 30% Glass Reinforced Information provided by FIBERFIL Engineered Plastics |
|||
Flexural Strength | 107 MPa | 15500 psi | ASTM D790 |
KYDEX® FST Fully Compliant Aviation Thermoforming Sheet KYDEX® FST meets all fire, smoke and heat release requirements set forth by the Federal Aviation Regulations 25.853 paragraphs (a) and (d) as well as toxicity requirements for ABD0031, BSS7239 an.. |
|||
Flexural Strength | 107 MPa | 15500 psi | 1.3 mm/min, 50 mm span; ASTM D790 |
SABIC Innovative Plastics LNP LUBRICOMP KFL23LH Acetal Copolymer LNP LUBRICOMP* KFL23LH is a compound based on Acetal Copolymer resin containing 15% Glass Fiber, 10% PTFE. Added features of this material include: Wear Resistant, Low Extractable. |
|||
Flexural Strength | 107 MPa | 15500 psi | 1.3 mm/min, 50 mm span; ASTM D790 |
SABIC Innovative Plastics LNP LUBRICOMP KFL36 Acetal Copolymer (Asia Pacific) LNP* Lubricomp* KFL36 is a compound based on Acetal Copolymer resin containing Glass Fiber, PTFE. Added features of this material include: Internally Lubricated. |
|||
Flexural Strength | 107 MPa | 15500 psi | 1.3 mm/min, 50 mm span; ASTM D 790 |
SABIC Innovative Plastics LNP Lubricomp KFL36XXC Acetal Copolymer (Europe-Africa-Middle East) LNP* Lubricomp* KFL36 is an Acetal containing Glass Fiber and PTFE.This data was supplied by SABIC-IP for the Europe-Africa-Middle East region. |
|||
Flexural Strength | 107 MPa | 15500 psi | ISO 178 |
SABIC Innovative Plastics LNP LUBRICOMP RAL23S PA 66 LNP LUBRICOMP* RAL23S is a compound based on Nylon 66 resin containing 10% PTFE, 15% Aramid. Added features of this material include: Heat Stabilized, Wear Resistant. |
|||
Flexural Strength | 107 MPa | 15500 psi | ASTM D790 |
Techmer ES HiFill® PP CO GF30 CC 30% Glass Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber Reinforcement, 30% Filler by WeightFeatures: Copolymer and Chemically CoupledInformation provided by TP Composites, Inc. |
|||
Flexural Strength | 107 MPa | 15500 psi | ASTM D790 |
Chase Plastics CP Pryme® N100HSL (DAM) Nylon 6, Heat Stabilized, Internally Lubricated Information provided by Chase Plastics. |
|||
Flexural Strength | 107 MPa | 15500 psi | ASTM D790 |
Chase Plastics CP Pryme® N100L (DAM) Nylon 6, Internally Lubricated Information provided by Chase Plastics. |
|||
Flexural Strength | 107 MPa | 15500 psi | ASTM D790 |
Westlake Plastics Zelux® CN-P Polycarbonate (conductive) Carbon-powder-filled with high flexural strength and good thermal stability to 275F. The CN-P is UL94 V-0 rated at 0.030" and is thermoformable in thinner gauges (0.010"-0.060").Information provide.. |
|||
Flexural Strength | 107 MPa | 15500 psi | ASTM D790 |
Westlake Plastics Zelux® SD-P Polycarbonate (static dissipative) Carbon powder filled with high flexural strength and good thermal stability to 270°F. Thermoformable in 0.010" to 0.060" gauges; low outgassing.Information provided by Westlake Plastics. |
|||
Flexural Strength | 107 MPa | 15500 psi | ISO 178 |
Polyplastics Duranex® 7307B Polybutylene Terephthalate (PBT), Super low warpage, GB filled DURANEX® is a crystalline thermoplastic based on polybutylene terephthalate (PBT) that can be readily strengthened, modified, or otherwise performance enhanced through the addition of glass fibers .. |
|||
Flexural Strength | 107 MPa | 15500 psi | ISO 178 |
Azoty Tarnow™ TARNOFORM 300 GF2 GB2 POM 10% glass fiber/10% glass beads mix reinforced injection molding grade, suitable for applications where increased strength and stiffness is required with care of the surface quality.Information prov.. |
|||
Flexural Strength | 107 MPa | 15500 psi | ISO 178 |
Azoty Tarnow™ TARNOFORM 300 GF2 POM 10% glass fiber reinforced injection molding grade, suitable for applications where increased strength and stiffness is required.Information provided by Zakłady Azotowe w Tarnowie-Moscicach S.A... |
|||
Flexural Strength | 107 MPa | 15500 psi | 23°C, 50% RH; ASTM D790 |
Asahi Kasei Xyron® SZ800 Modified Polyphenylene Ether High-Heat ResistantInformation provided by Asahi Kasei |
|||
Flexural Strength | 107 MPa | 15500 psi | ASTM D790 |
A. Schulman ComAlloy Hiloy® 132 Polypropylene, Glass/Mineral Reinforced, Chemically Coupled Data provided by the manufacturer, ComAlloy International Company.45% Glass/Mineral Reinforced.The ComAlloy product line has been integrated into the A Schulman product line. |
|||
Flexural Strength | 107 MPa | 15500 psi | 2mm/min; ASTM D790 |
Denka TX-100S Transparent Resin Polymer (MS resin) Methyl Methacrylate Styrene "TX Polymer" (methyl methacrylate styrene), MS resins as an alternative to acrylic resins, with low density, low moisture absorption, and good moldability, "TH Polymer/TP Polymer," MBS resins with a.. |
|||
Flexural Strength | 107 MPa | 15500 psi | 23°C, 50% RH; ASTM D790 |
Asahi Kasei Xyron® 740V Modified Polyphenylene Ether Flame RetardantInformation provided by Asahi Kasei |
|||
Flexural Strength | 107 MPa | 15500 psi | ISO 178 |
Ascend Performance Materials Vydyne® ECO366 Nylon 66, Flame-retardant, DAM Vydyne® ECO366 is a non-halogenated, unfilled, flame-retardant PA66 homopolymer designed with superior flow properties to assist in filling thin-walled, intricate parts. It is lubricated for machin.. |