Mechanical Properties Metric English Comments
Flexural Strength 107.7 MPa
15620 psi
ASTM D790M-93
Propex Fabrics Curv™ C100A Polypropylene/Polypropylene Thermoformable Composite
Curv™ key features include weight savings, total recyclability, no glass content, thermoformable, high impact strength, inertness, and abrasion resistance.Data provided by BP Amoco; Curv was spun o..