Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Strength | 107.91 MPa | 15651 psi | |
Shinil Chemical SHINSTAT PC Electrostatic Control Polymer Injection Grade SHINSTAT is an Inherently Dissipative Polymer (IDP) compound which can discharge the electrostatic charge (ESD) effectively. Shinil has designed SHINSTAT using Shinil's patented IDP technology for .. |
|||
Flexural Strength | 107.91 MPa | 15651 psi | ASTM D790 |
E-Polymers TEKAFIN® PH50G2 20% Glass Fiber Reinforced High Strength Compounded-PP Modified PP: TEKAFIN is modified PP resins formulated with various fillers and modifiers. It has product lines for impact modified, glass fiber reinforced, inorganic filler reinforced and hybrids.I.. |
|||
Flexural Strength | 107.91 MPa | 15651 psi | ASTM D790 |
E-Polymers TEKAMID® JN110 PPE+PA66 Filler Reinforced PA/PPE Alloy Polyamide (Nylon) Resin. TEKAMID is widely being used in manufacturing of automotive and industrial parts with its outstanding mechanical, thermal and chemical properties.JN-series: PA66/PPE, PA6/P.. |
|||
Flexural Strength | 107.91 MPa | 15651 psi | ASTM D790 |
E-Polymers TEKAPPO® JF6 Un-Reinforced Flame Retardant Heat Resistance M-PPO Modified PPO/PPE: TEKAPPO is a modified PPO/PPE, blending PPO with HIPS in order to improve HDT and processability. It displays various HDT range with halogen-free flammability, impact resistance a.. |
|||
Flexural Strength | 107.91 MPa | 15651 psi | ASTM D790 |
E-Polymers TEKAMID® H12TW Unreinforced Low warpage PA/ABS Alloy Polyamide (Nylon) Resin. TEKAMID is widely being used in manufacturing of automotive and industrial parts with its outstanding mechanical, thermal and chemical properties.H-series: PA6/ABS, PA66/AB.. |