Polymer Property : Flexural Strength = 1570 psi Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Flexural Strength 10.8 MPa
1570 psi
ASTM D790
A. Schulman POLYFORT™ PP 3720
Information provided by A. Schulman.
Flexural Strength 10.8 MPa
1570 psi
ASTM D790
A. Schulman POLYFORT™ PP 3720
Information provided by A. Schulman.
Flexural Strength 10.8 MPa
1570 psi
ASTM D790
A. Schulman POLYFORT™ PP 3720
Information provided by A. Schulman.
Flexural Strength 10.8 MPa
1570 psi
ASTM D790
A. Schulman POLYFORT™ PP 3720
Information provided by A. Schulman.
Flexural Strength 10.8 MPa
1570 psi
ASTM D790
A. Schulman POLYFORT™ PP 3720
Information provided by A. Schulman.
Flexural Strength 10.8 MPa
1570 psi
ASTM D790
A. Schulman POLYFORT™ PP 3720
Information provided by A. Schulman.