Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Flexural Strength 1600 MPa
232000 psi
SGL Carbon Group SIGRAFIL C® in 250°F Epoxy
60% fiber volumeInformation provided by SGL Carbon Group
Flexural Strength 1600 MPa
232000 psi
China Tungsten NT4 Titanium Carbonitride Alloy
Titanium carbonitride base alloy , also called cermets, with of high hardness, good red hard-ness and wear resistance, medium toughness, high  corrosion resistance to acids and alkalis and hi-tempe..
Flexural Strength 1600 MPa
232000 psi
China Tungsten YG3X Tungsten Carbide for Cutting Tools
Best wear resistance among W-Co alloys yet impact toughness comparatively low, High speed finishing of small chip section of cast irons, non-ferrous metals & alloys quenched steel and alloy steel.In..
Flexural Strength 1600 MPa
232000 psi
China Tungsten ZK10-1 Tungsten Carbide
Semi-finishing and finishing of cast iron and machining of cat alloy iron, bronze and copper. Suitable for machining of aluminum and aluminum alloysInformation provided by China Tungsten
Flexural Strength 1600 MPa
232000 psi
China Tungsten ZC1 Tungsten Carbide
Coated substrate of higher toughness and red hardness, for semi-finishing or finishing of carbon steel and alloy steel, generally for threading toolsInformation provided by China Tungsten
Flexural Strength 1600 MPa
232000 psi
Bending Strength; 4-Point; DIN ENV 843-1
CeramTec ATZ Alumina Toughened Zirconia, Dental Grade
ATZ is an alumina toughened zirconia used in dental applications.