Mechanical Properties Metric English Comments
Flexural Strength 163.83 MPa
23762 psi
ASTM D790
E-Polymers SEPAZ® N6000FR Nanoclay 4% Flame Retardant Nano Composite Resin
Nanocomposite: SEPAZ Nano PA6 nanocomposites have been prepared successfully in commercial scale through 'in situ' polymerization or melt extrusion. The unique performance properties of nanocomposi..
Flexural Strength 163.83 MPa
23762 psi
ASTM D790
E-Polymers SEPAZ® C140GM 40% Glass Fiber/Mineral Reinforced LCP Resin
Liquid Crystal Polymer Resin: SEPAZ LCP resin has a unique structure and performance unthought of in a traditional plastics. Beside SEPAZ LCP takes the excels in all-around performance and molding ..