Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Strength | 112.4 MPa | 16300 psi | LW; ASTM D790 |
Haysite H208 Polyester, Magnetic Permeable Grade H208 has high magnetic permeability and excellent retention of properties after heat aging at elevated temperatures. This unique combination of properties allows Grade H208 to be used in vari.. |
|||
Flexural Strength | 112 MPa | 16300 psi | ASTM D790 |
Techmer ES HiFill® PA6/6 0177 B Nylon 66 Availability: North AmericaForms: PelletsFiller/Reinforcement: Barium SulfateFeatures: High Specific GravityInformation provided by TP Composites, Inc. |
|||
Flexural Strength | 112 MPa | 16300 psi | ASTM D790 |
Techmer ES Luriblend® PA6 ML2 HS BK Nylon 6 Availability: North AmericaForms: PelletsAdditive: Heat Stabilizer and Molybdenum Disulfide Lubricant(2%)Features: Good Wear Resistance, Low Friction, Heat Stabilized and LubricatedAppearance: Blac.. |
|||
Flexural Strength | 112 MPa | 16300 psi | ASTM D790 |
Techmer ES Luriblend® PA6 ML3 BK Nylon 6 Availability: North AmericaForms: PelletsAdditive: Heat Stabilizer and Molybdenum Disulfide Lubricant(3%)Features: Good Wear Resistance, Low Friction, Heat Stabilized and LubricatedAppearance: Black.. |
|||
Flexural Strength | 112 MPa | 16300 psi | ASTM D790 |
Asahi Kasei Thermylene® P-25FG-3809 25% Glass Fiber Reinforced Information provided by Asahi Thermofil |