Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Strength | 115.5 MPa | 16750 psi | ASTM D790 |
Quadrant EPP Semitron® MP-370 (ASTM Product Data Sheet) |
|||
Flexural Strength | 115.5 MPa | 16750 psi | ASTM D790 |
PolyOne Edgetek® ATH-25GF/000 Acetal-Homopolymer, Glass Filled
(discontinued **) Description/Features:Glass Fiber ReinforcedUL 94 HBPolyOne First ChoiceInformation provided by PolyOne Corporation. |