Mechanical Properties Metric English Comments
Flexural Strength 176.58 MPa
25611 psi
Shinil Chemical SHINCON PC Electro Conductive Polymer
SHINCON is the product line of SHINIL's electrically conductive compound which is able to dissipate the electrostatic charge (ESD) effectively. Shinil has developed SHINCON products using Shinil's ..
Flexural Strength 176.58 MPa
25611 psi
Shinil Chemical SHINFLAME PC/PBT GF Flame Retardant Polymer Appliance
SHINFLAME is a flame retardant (FR) compound which exhibits inherent flame retardant properties during fire. Shinil uses its patented dispersion blending technology with variety of polymers to prod..
Flexural Strength 176.58 MPa
25611 psi
Shinil Chemical SHINNANO PA-66 Polymer Nanocomposite Engine Cover
SHINNANO is the product line of polymer nanocomposite made by dispersing nano fillers, mainly, NANOCLAY. Recently, Shinil has developed varios nanocomposite grades for automotive applications using..