Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Strength | 181.49 MPa | 26323 psi | ASTM D790 |
E-Polymers SEPAZ® LC50 PP Copolymer LFT Resin Long Fiber Thermoplastics: SEPAZ LFT products, injection moldable long fiber-reinforced thermoplastics (LFT), are made using a unique pultrusion that thoroughly wets out the glass fibers and deliver.. |
|||
Flexural Strength | 181.49 MPa | 26323 psi | ASTM D790 |
E-Polymers SEPAZ® LH40 PP Homopolymer LFT Resin Long Fiber Thermoplastics: SEPAZ LFT products, injection moldable long fiber-reinforced thermoplastics (LFT), are made using a unique pultrusion that thoroughly wets out the glass fibers and deliver.. |
|||
Flexural Strength | 181.49 MPa | 26323 psi | ASTM D790 |
E-Polymers SEPAZ® V220A 20% Glass Fiber Reinforced PPA Polyphthal Amide Resin (High Temperature Nylon): SEPAZ PPA is a unique semi-crystalline engineering plastic that bridges the cost-performance gap between traditional engineering thermoplastics and s.. |
|||
Flexural Strength | 181.49 MPa | 26323 psi | ASTM D790 |
E-Polymers TEKASTER® F10G30 30% Glass Fiber Reinforced PBT Polyester Resin: TEKASTER is thermoplastic polyester resins (PBT, PET) mostly injection molding. PBT has excellent mechanical properties and well balanced engineering plastics with an electrical pe.. |
|||
Flexural Strength | 181.49 MPa | 26323 psi | ASTM D790 |
E-Polymers SEPAZ® C240GM 40% Glass Fiber/Mineral Reinforced LCP Resin Liquid Crystal Polymer Resin: SEPAZ LCP resin has a unique structure and performance unthought of in a traditional plastics. Beside SEPAZ LCP takes the excels in all-around performance and molding .. |