Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Strength | 1300 MPa | 189000 psi | Transverse Rupture |
Pacific Sintered Materials FX-232-T(HT) Infiltrated High Carbon Steel Powdered Metal Good strength, shock resistance and hardenability. Moderate tolerance control.Equivalent MPIF Specification: FX-1008-110HTAll information provided by Pacific Sintered Metals. |
|||
Flexural Strength | 1300 MPa | 189000 psi | Transverse Rupture |
PSM Industries Pacific Sintered Metals Infiltrated High Carbon Steel FX-232-T(HT) Powdered Metal Good strength, shock resistance and hardenability, Moderate tolerance control Equivalent MPIF Specification: FX-1008-110HTInformation Provided by Pacific Sintered Metals, a division of PSM Industri.. |
|||
Flexural Strength | 1300 MPa | 189000 psi | |
MarkeTech Zirconium Oxide Ceramic Zirconia, Tetragonal, Y2O3 Stabilized Data provided by the supplier, MarkeTech International.Zirconium oxide is widely used and has superior high temperature properties. When combined with yttria the strength and fracture toughness is .. |
|||
Flexural Strength | <= 1300 MPa | <= 189000 psi | 4-point |
Wieland Zeno™ Zr Disc Zirconium Oxide Zirconium oxide blanks supplied partly sintered. Available in five different thicknesses to reduce material costs. Applications: modern dental restorationsDental |
|||
Flexural Strength | 1300 MPa | 189000 psi | |
China Tungsten NT5 Titanium Carbonitride Alloy Titanium carbonitride base alloy , also called cermets, with of high hardness, good red hard-ness and wear resistance, medium toughness, high corrosion resistance to acids and alkalis and hi-tempe.. |