Polymer Property : Flexural Strength = 19004 psi Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Flexural Strength 131.03 MPa
19004 psi
ASTM D790
Lucent Polymers GPB-115 Polybutylene Terephthalate, 15% Glass Fiber Reinforced
Add "R" for Added ReleaseAdd "U" for UV StabilizerInformation provided by Lucent Polymers, Inc.
Flexural Strength 131.03 MPa
19004 psi
ASTM D790
Lucent Polymers GPCB-110 Polycarbonate+PBT, 10% Glass Fiber Reinforced
Add "R" for Added ReleaseAdd "U" for UV StabilizerInformation provided by Lucent Polymers, Inc.