Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Strength | 132 MPa | 19200 psi | ASTM D790 |
Techmer ES Electrablend® ABS CF10 FR BK 10% Carbon Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Carbon Fiber, 10% Filler by WeightFeatures: Flame RetardantAppearance: BlackInformation provided by TP Composites, Inc. |
|||
Flexural Strength | 132 MPa | 19200 psi | ASTM D790 |
Chase Plastics CP Pryme® N340HSL (COND, 50% RH) Nylon 6 (Utility Grade), 40% Glass Fiber Reinforced, Heat Stabilized, Internally Lubricated Information provided by Chase Plastics. |
|||
Flexural Strength | 132 MPa | 19200 psi | ASTM D790 |
Ensinger Tecapeek® XP-181 Compression Molded PPEK Compound, EWS Filled and Carbon Fiber Reinforced Ensinger Special Polymers offers over twenty different VICTREX® PEEK blends to choose from and has the capability to blend custom compounds for specific applications. Compression molding results in.. |