Mechanical Properties Metric English Comments
Flexural Strength 194.24 MPa
28172 psi
ASTM D790
E-Polymers TEKAMID® JN930 PPE+PA66 30% Glass Fiber Reinforced PA/PPE Alloy
Polyamide (Nylon) Resin. TEKAMID is widely being used in manufacturing of automotive and industrial parts with its outstanding mechanical, thermal and chemical properties.JN-series: PA66/PPE, PA6/P..
Flexural Strength 194.24 MPa
28172 psi
ASTM D790
E-Polymers TEKAMID® JN920 PPE+PA66 20% Glass Fiber Reinforced PA/PPE Alloy
Polyamide (Nylon) Resin. TEKAMID is widely being used in manufacturing of automotive and industrial parts with its outstanding mechanical, thermal and chemical properties.JN-series: PA66/PPE, PA6/P..