Polymer Property : Flexural Strength = 194.5 MPa Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Flexural Strength 194.5 MPa
28210 psi
ISO 178
Polyplastics Duranex® CRN7030 Polybutylene Terephthalate (PBT), Low gas generation, Low contact contamination, FR, UL approved regrind 50%, 30% GF filled
DURANEX® is a crystalline thermoplastic based on polybutylene terephthalate (PBT) that can be readily strengthened, modified, or otherwise performance enhanced through the addition of glass fibers ..