Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Strength | 1400 MPa | 203000 psi | DIN EN 843-1 |
CeramTec MZ 111 HIP Zirconia, ZrO2-Y2O3 MZ 111 HIP is a yttria-stabilized tetragonal zirconia ceramic. |
|||
Flexural Strength | 1400 MPa | 203000 psi | Bending Strength; 4-Point; without HIP: 1050; DIN ENV 843-1 |
CeramTec MZ 111 Zirconia, ZrO2-Y2O3 MZ 111 is a yttria-stabilized tetragonal zirconia used in dental applications. |