Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Strength | 1.52 MPa | 220 psi | ISO 178 |
PolyOne Nymax™ GF 600 A 33 HS7 DX9 Black Polyamide 6 (Nylon 6) The Nymax® GF 600 Series of glass fiber-reinforced nylon 6 compounds have been specifically engineered for applications requiring high stiffness, tensile strength, and toughness, while providing en.. |
|||
Flexural Strength | 1.52 MPa | 220 psi | at 5% deflection; ASTM D790 |
DSM Biomedical PurSil® 20 Thermoplastic Silicone Polyether Polyurethane (TSPU) A novel copolymer that is strong yet flexible with proven biocompatibility and biostability
Combining the benefits of both silicone elastomers and polyether urethanes, PurSil® TSPU has exceptional.. |