Mechanical Properties Metric English Comments
Flexural Strength 156.96 MPa
22765 psi
Shinil Chemical SHINCON PSU-CNT LCD Rack
LCD Rack is used to transfer or bake LCD frame in the electronic assembly or LCD packaging assembly line. Current LCD Rack is made of poly ether ether ketone (PEEK) with carbon fiber (CF). Since b..
Flexural Strength 156.96 MPa
22765 psi
Shinil Chemical SHINSTRA PBT SBV1015 Structural Polymer Lamp Housing
SHINSTRA is the product line of structural polymer compound which exhibits excellent physical, mechanical, and thermal properties. Shinil uses the state-of-the-art dispersion and blending technolog..
Flexural Strength 156.96 MPa
22765 psi
ASTM D790
E-Polymers SEPAZ® N1140 Nanoclay 4% Medium Viscosity Nano Composite Resin
Nanocomposite: SEPAZ Nano PA6 nanocomposites have been prepared successfully in commercial scale through 'in situ' polymerization or melt extrusion. The unique performance properties of nanocomposi..
Flexural Strength 156.96 MPa
22765 psi
ASTM D790
E-Polymers SEPAZ® V200L Unfilled PPA
Polyphthal Amide Resin (High Temperature Nylon): SEPAZ PPA is a unique semi-crystalline engineering plastic that bridges the cost-performance gap between traditional engineering thermoplastics and s..
Flexural Strength 156.96 MPa
22765 psi
ASTM D790
E-Polymers TEKAPPO® J930 30% Glass Fiber Reinforced M-PPO
Modified PPO/PPE: TEKAPPO is a modified PPO/PPE, blending PPO with HIPS in order to improve HDT and processability. It displays various HDT range with halogen-free flammability, impact resistance a..
Flexural Strength 156.96 MPa
22765 psi
ASTM D790
E-Polymers TEKAPPO® JF201 Filler Reinforced Heat Resistant Dimensional Stability Flame Retardant M-PPO
Modified PPO/PPE: TEKAPPO is a modified PPO/PPE, blending PPO with HIPS in order to improve HDT and processability. It displays various HDT range with halogen-free flammability, impact resistance a..
Flexural Strength 156.96 MPa
22765 psi
ASTM D790
E-Polymers TEKASTER® F10G30H 30% Glass Fiber Reinforced Impact Modified PBT
Polyester Resin: TEKASTER is thermoplastic polyester resins (PBT, PET) mostly injection molding. PBT has excellent mechanical properties and well balanced engineering plastics with an electrical pe..
Flexural Strength 156.96 MPa
22765 psi
ASTM D790
E-Polymers SEPAZ® LH30 PP Homopolymer LFT Resin
Long Fiber Thermoplastics: SEPAZ LFT products, injection moldable long fiber-reinforced thermoplastics (LFT), are made using a unique pultrusion that thoroughly wets out the glass fibers and deliver..