Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Strength | 15.9 MPa | 2300 psi | |
UCAR Carbon UCAR® CHV Extruded Graphite Typical uses for extruded grades are in the production of molds and crucibles, heating elements and furnace furniture, liquid metal processing equipment and chemical process equipment.Tabular proper.. |
|||
Flexural Strength | 15.9 MPa | 2300 psi | ASTM D-790 |
CMT Materials REN Shape® 440 Tooling Board, Modeling Board, Adhesive Products CMT Materials offers the complete line of REN Shape tooling board, modeling board, and related adhesive products. Vacuum formers and thermoformers use these products as prototype and low volume prod.. |
|||
Flexural Strength | 15.86 MPa | 2300 psi | |
Pyrotek Pyroboard™ S800 Roller Pyroboard™ S800 is used in cooling areas of the furnace. Economically priced, S800 wears well and is designed to be used in the water quench cooling sections.Information provided by Pyrotek. |