Polymer Property : Flexural Strength = 242 MPa Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Flexural Strength 242 MPa
35100 psi
ISO 178
PolyOne Nymax™ GF 600 A 33 Natural Polyamide 6 (Nylon 6)
The Nymax® GF 600 Series of glass fiber-reinforced nylon 6 compounds have been specifically engineered for applications requiring high stiffness, tensile strength, and toughness, while providing en..
Flexural Strength 242 MPa
35100 psi
Lushan PA66 + 30% GF Nylon Toughener/PA Impact Modifier
Nylon toughener/PA impact modifier Lushan series is a maleic anhydride grafted polyolefin elastomer, with a very low residual maleic anhydride monomer, no irritating odor when using. Nylon toughener..
Flexural Strength 242 MPa
35100 psi
GB/T 9341-2008
Sichuan Deyang Haton® hGR30 Polyphenylene Sulfide, Glass Fiber Reinforced
Injection moldingInformation provided by Sichuan Deyang Chemical Co., LTD
Flexural Strength 242 MPa
35100 psi
1.3 mm/min, 50 mm span; ASTM D790
SABIC Innovative Plastics LNP THERMOCOMP RF006 PA 66
LNP* THERMOCOMP* RF006 is a compound based on Nylon 66 resin containing 30% Glass Fiber.
Flexural Strength 242 MPa
35100 psi
1.3 mm/min, 50 mm span; ASTM D790
SABIC Innovative Plastics LNP THERMOCOMP RF006S PA 66
LNP* THERMOCOMP* RF006S is a compound based on Nylon 66 resin containing 30% Glass Fiber. Added features of this material include: Heat Stabilized.
Flexural Strength 242 MPa
35100 psi
1.3 mm/min, 50 mm span; ASTM D790
SABIC Innovative Plastics LNP THERMOCOMP RF006XXH PA 66
LNP* THERMOCOMP* RF006XXH is a compound based on Nylon 66 resin containing 30% Glass Fiber. Added feature of this material is: Healthcare.
Flexural Strength 242 MPa
35100 psi
ASTM D790
Ashley Polymers Ashlene® 528L-30G Nylon 66, 30% Glass Reinforced
General purpose glass fiber reinforced Nylon 66 designed for parts requiring excellent thermal and dimensional stability and higher strength than conventional resins.Data provided by the manufacture..
Flexural Strength 242 MPa
35100 psi
ASTM D790
Ashley Polymers Ashlene® 528L-30LG Nylon 66, 30% Long Glass Fiber Reinforced
Long glass fiber reinforced Nylon 66 designed for parts requiring excellent thermal and dimensional stability and higher strength than available with conventional glass reinforced resins.Data provid..
Flexural Strength 242 MPa
35100 psi
ASTM D790
A. Schulman ComAlloy Hiloy® 623 Nylon 6/6, Glass Reinforced, Flow Enhanced, UL
Data provided by the manufacturer, ComAlloy International Company.33% Glass Reinforced.The ComAlloy product line has been integrated into the A Schulman product line.