Polymer Property : Flexural Strength = 252 psi Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Flexural Strength 1.74 MPa
252 psi
Parallel to thickness
Zircar Zirconia ZYZ-6 Zirconia Boards and Discs Insulation
Type ZYZ Boards and Discs are rigid, refractory structures composed of yttria-stabilized zirconia fibers that are bonded with silica. This unique composition provides Type ZYZ insulation with the lo..
Flexural Strength 1.74 MPa
252 psi
Parallel to thickness
Zircar Zirconia ZYZ-6 Zirconia Boards and Discs Insulation
Type ZYZ Boards and Discs are rigid, refractory structures composed of yttria-stabilized zirconia fibers that are bonded with silica. This unique composition provides Type ZYZ insulation with the lo..