Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Strength | 17.5 MPa | 2540 psi | After conditioning at 23°C and 50% RH; ISO 178 |
Arkema Group Orgalloy® LE 60XV Polyamide 6 Alloy Polyamide Alloy, Semi-Flexible grade, Nylon 6 basedTubes / Mandrels / Profiles / CablesInformation provided by Arkema Group |