Polymer Property : Flexural Strength = 26600 psi Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Flexural Strength 183 MPa
26600 psi
ASTM D790
PolyOne Edgetek® PF-40GF/000 Polysulfone, Glass Filled  (discontinued **)
Description/Features:Glass Fiber ReinforcedUL 94 V0PolyOne First ChoiceInformation provided by PolyOne Corporation.