Polymer Property : Flexural Strength = 2700 MPa Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Flexural Strength 2300 - 2700 MPa
334000 - 392000 psi
China Tungsten Z25 Tungsten Carbide for Mining Purposes
Of high toughness and wear resistance as well as good versatility, for rotary hammer rock drill bits and pillar bit drills, for f14~f16 medium hard and hard rock formations.Information provided by C..