Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Strength | 284 MPa | 41200 psi | ASTM D790 |
Kolon KOPA® KN333G30HS G/F Reinforced Nylon 66 High thermal resistant, high strength, dimensionally stableApplications Transmission gear supportersInformation provided by API-Kolon. |
|||
Flexural Strength | 284 MPa | 41200 psi | ASTM D790 |
Kolon KOPA® KN333G35CR G/F Reinforced Nylon 66 High thermal resistant, Weather resistant, dimensionally stableApplications Cylinder head coversInformation provided by API-Kolon. |
|||
Flexural Strength | 284 MPa | 41200 psi | ISO 178 |
SABIC Innovative Plastics LNP LUBRICOMP EX03647H PEI LNP LUBRICOMP* EX03647H is a compound based on Polyetherimide resin containing Proprietary Fillers. Added features of this material include: Healthcare, Wear Resistant. |
|||
Flexural Strength | 284 MPa | 41200 psi | ISO 178 |
SABIC Innovative Plastics LNP THERMOCOMP IC006 PA 6/12 LNP* THERMOCOMP* IC006 is a compound based on Nylon 6/12 resin containing 30% Carbon Fiber. Added features of this material include: Electrically Conductive. |
|||
Flexural Strength | 284 MPa | 41200 psi | ISO 178 |
SABIC Innovative Plastics LNP THERMOCOMP IC006 PA 6/12 (Asia Pacific) LNP* Thermocomp* IC006 is a compound based on Nylon 6/12 resin containing Carbon Fiber. Added features of this material include: Electrically Conductive. |
|||
Flexural Strength | 284 MPa | 41200 psi | ISO 178 |
SABIC Innovative Plastics LNP THERMOCOMP VC006 SUPER TOUGH NYLON LNP* THERMOTUF* VC006 is a compound based on Super Tough Nylon resin containing 30% Carbon Fiber. Added features of this material include: High Impact, Electrically Conductive. |
|||
Flexural Strength | 284 MPa | 41200 psi | ISO 178 |
SABIC Innovative Plastics LNP THERMOTUF VC006 Super Tough PA 6/6 LNP* THERMOTUF* VC006 is a compound based on Super Tough Nylon 6/6 resin containing Carbon Fiber. Added features of this material include: High Impact. |
|||
Flexural Strength | 284 MPa | 41200 psi | 1.3 mm/min, 50 mm span; ASTM D790 |
SABIC Innovative Plastics LNP THERMOCOMP RF007SXN PA 66 LNP* THERMOCOMP* RF007SXN is a Hydro-Stable, 35% Glass Fiber reinforced compound based on Nylon 66. Added features of this grade include: Heat Stabilized, NSF Listed. |
|||
Flexural Strength | 284 MPa @Temperature 23.0 °C |
41200 psi @Temperature 73.4 °F |
ISO 178 |
Solvay Specialty Polymers Amodel® AS-1566 HS Polyphthalamide (PPA)
(Unverified Data**) Amodel AS-1566 HS resin is a 65% glass and mineral reinforced polyphthalamide (PPA) resin that exhibits a high deflection temperature and high flexural modulus. This grade was designed specifically .. |