Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Strength | 299 MPa | 43400 psi | 2.8mm/min; ASTM D790 |
Asia International Enterprise (Hong Kong) 60G8 Nylon 66, 40% Filled Information provided by Asia International Enterprise (Hong Kong) Ltd. |