Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Strength | 24.0 - 30.0 MPa | 3480 - 4350 psi | ASTM D790M |
DSM Somos® 9420 Epoxy Resin for Stereolithography DescriptionDSM Somos® 9420 is a liquid photopolymer that produces robust, functional and accurate parts using stereolithography machines. The material offers superior chemical resistance and a wid.. |