Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Strength | 138 - 207 MPa @Strain 5.00 % |
20000 - 30000 psi @Strain 5.00 % |
ASTM D790 |
Arkema Group KYNAR® 370 Polyvinylidene Fluoride (PVDF) Homopolymer - Injection Molding Characteristics: Natural resin - translucent, off-white hemispheres. Low melt shrinkage, graphite powder filled. High stability in harsh thermal, chemical and ultraviolet environments. High toug.. |