Mechanical Properties Metric English Comments
Flexural Strength 2.10 MPa
305 psi
Parallel to thickness
Zircar Zirconia ZYFB-6 Zirconia Boards, Discs, and Cylinders Insulation
Type ZYFB Boards, Discs and Cylinders are rigid, refractory structures composed of yttria-stabilized zirconia fibers that do not undergo the usual phase transitions associated with pure zirconia. Ty..
Flexural Strength 2.10 MPa
305 psi
@ 15 kg/m<sup>2</sup>; ASTM DC201
Samsung Cheil Industries Starex® SF-200H Expandable Polystyrene (EPS) FR
Characteristics: High Strength, High ExpansionTypical Application : InsulationInformation provided by Samsung Cheil Industries.
Flexural Strength 2.10 MPa
305 psi
@ 15 kg/m<sup>2</sup>; ASTM DC201
Samsung Cheil Industries Starex® SF-200H Expandable Polystyrene (EPS) FR
Characteristics: High Strength, High ExpansionTypical Application : InsulationInformation provided by Samsung Cheil Industries.
Flexural Strength 2.10 MPa
305 psi
Parallel to thickness
Zircar Zirconia ZYFB-6 Zirconia Boards, Discs, and Cylinders Insulation
Type ZYFB Boards, Discs and Cylinders are rigid, refractory structures composed of yttria-stabilized zirconia fibers that do not undergo the usual phase transitions associated with pure zirconia. Ty..