Mechanical Properties Metric English Comments
Flexural Strength 32.8 MPa
4750 psi
UCAR Carbon UCAR® ATJ Isostatic Molded Graphite
Isostatically molded ATJ has been an industry standard for many years. It is a fine grain, high strength material which can be machined to precise tolerances and a fine surface finish. Grade ATJ has..