Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Strength | 225 MPa | 32700 psi | ASTM D790 |
Techmer ES Plastiblend® PA6 GF20 RM-B L NAT Nylon 6 Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber Reinforcement, 20% Filler by WeightAdditive: LubricantFeatures: Low Moisture Absorption and LubricatedAppearance: BlackTPCI.. |
|||
Flexural Strength | 225 MPa | 32700 psi | ASTM D790 |
A. Schulman SCHULAMID® 66 GF33 33% Glass Fiber Reinforced Nylon 66 Information provided by A. Schulman. |
|||
Flexural Strength | 225 MPa | 32700 psi | ASTM D790 |
A. Schulman SCHULAMID® 66 GF33H 33% Glass Fiber Reinforced, Heat Stabilized Nylon 66 Information provided by A. Schulman. |
|||
Flexural Strength | 225 MPa | 32700 psi | ASTM D790 |
Chase Plastics CP Pryme® NN143GL (COND, 50% RH) Nylon 66, 43% Glass Fiber Reinforced, Internally Lubricated Information provided by Chase Plastics. |
|||
Flexural Strength | 225 MPa | 32700 psi | ASTM D790 |
A. Schulman SCHULAMID® 66 GF33 33% Glass Fiber Reinforced Nylon 66 Information provided by A. Schulman. |
|||
Flexural Strength | 225 MPa | 32700 psi | ASTM D790 |
A. Schulman SCHULAMID® 66 GF33H 33% Glass Fiber Reinforced, Heat Stabilized Nylon 66 Information provided by A. Schulman. |
|||
Flexural Strength | 225 MPa | 32700 psi | ASTM D790 |
A. Schulman SCHULAMID® 66 GF33 33% Glass Fiber Reinforced Nylon 66 Information provided by A. Schulman. |
|||
Flexural Strength | 225 MPa | 32700 psi | ASTM D790 |
A. Schulman SCHULAMID® 66 GF33H 33% Glass Fiber Reinforced, Heat Stabilized Nylon 66 Information provided by A. Schulman. |
|||
Flexural Strength | 225 MPa | 32700 psi | ASTM D790 |
A. Schulman SCHULAMID® 66 GF33 33% Glass Fiber Reinforced Nylon 66 Information provided by A. Schulman. |
|||
Flexural Strength | 225 MPa | 32700 psi | ASTM D790 |
A. Schulman SCHULAMID® 66 GF33H 33% Glass Fiber Reinforced, Heat Stabilized Nylon 66 Information provided by A. Schulman. |
|||
Flexural Strength | 225 MPa | 32700 psi | ASTM D790 |
A. Schulman SCHULAMID® 66 GF33 33% Glass Fiber Reinforced Nylon 66 Information provided by A. Schulman. |
|||
Flexural Strength | 225 MPa | 32700 psi | ASTM D790 |
A. Schulman SCHULAMID® 66 GF33H 33% Glass Fiber Reinforced, Heat Stabilized Nylon 66 Information provided by A. Schulman. |
|||
Flexural Strength | 225 MPa | 32700 psi | ASTM D790 |
A. Schulman SCHULAMID® 66 GF33H 33% Glass Fiber Reinforced, Heat Stabilized Nylon 66 Information provided by A. Schulman. |
|||
Flexural Strength | 225 MPa | 32700 psi | ASTM D790 |
A. Schulman SCHULAMID® 66 GF33 33% Glass Fiber Reinforced Nylon 66 Information provided by A. Schulman. |