Mechanical Properties Metric English Comments
Flexural Strength 33.2 MPa
4820 psi
ASTM D790
Multibase Nylex™ 2185 R15 Polyamide + PP
Glass fiber reinforcement, 15% Filler by Weight. Features: Crack Resistance, GoodDimensional Stability, GoodImpact Resistance, GoodMoisture ResistantProcessability, GoodForms:PelletsProcessing Metho..