Polymer Property : Flexural Strength = 35571 psi Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Flexural Strength 245.25 MPa
35571 psi
Shinil Chemical SHINCON PES Electro Conductive Polymer
SHINCON is the product line of SHINIL's electrically conductive compound which is able to dissipate the electrostatic charge (ESD) effectively. Shinil has developed SHINCON products using Shinil's ..
Flexural Strength 245.25 MPa
35571 psi
Shinil Chemical SHINNANO PA-66 Polymer Nanocomposite Window Strip
SHINNANO is the product line of polymer nanocomposite made by dispersing nano fillers, mainly, NANOCLAY. Recently, Shinil has developed varios nanocomposite grades for automotive applications using..
Flexural Strength 245.25 MPa
35571 psi
ASTM D790
E-Polymers TEKALOY® F50G50 50% Glass Fiber Reinforced PBT/PET Alloy
PC/ABS, PC/PBT, PC/PET: TEKALOY is high performance polymer alloy resins (PC/ABS, PC/PBT, and PC/PET, etc) manufactured by E-Polymers. PC/ABS has excellent mechanical properties, high heat resistan..