Mechanical Properties Metric English Comments
Flexural Strength 36.3 MPa
5260 psi
ASTM D790
I. Stern HIPS SH03 High Impact Polystyrene
Features:High flowExcellent toughnessExcellent processabilityApplicationsInjection moldingAgency RatingsFDA Title 21 CFR 177.1640UL File E185934Information provided by I. Stern & Co. Inc.
Flexural Strength 36.3 MPa
5260 psi
2.8 mm/min; ASTM D790
Samsung Cheil Industries Starex® NH-1926 HIPS, Unreinforced FR
Non-halogen flame-retardant HIPS with high-impact that can be used in the exterior of TV and VCR interior/exterior material of OA devicesInformation provided by Samsung Cheil Industries.
Flexural Strength 36.3 MPa
5260 psi
2.8 mm/min; ASTM D790
Samsung Cheil Industries Starex® NH-1926 HIPS, Unreinforced FR
Non-halogen flame-retardant HIPS with high-impact that can be used in the exterior of TV and VCR interior/exterior material of OA devicesInformation provided by Samsung Cheil Industries.
Flexural Strength 36.3 MPa

@Thickness 3.20 mm
5260 psi

@Thickness 0.126 in
ASTM D790
Supreme Petrochem SH 03 High Impact Polystyrene
Characteristics High flow Good melt strength Excellent toughness Processing MoldingApplications Gas assisted injection molding of T.V. cabinets Suitable for thin walled parts, AC grills and toys ..